Blog

Fused Cast AZS Block Used In Different Parts Of Glass Furnace | glassonweb.com

The temperatures change from 1200℃ to 1600℃ during the whole process when the qualified glass is finished producing from material melting, and the glass liquid is in the convection state.  So different parts of glass furnace need different refractory bricks.

A. sidewall brick: sidewall is mainly adopted fused cast AZS block, and recently years fused cast α-β alumina is used in sidewall. Steel Fiber Castable

Fused Cast AZS Block Used In Different Parts Of Glass Furnace | glassonweb.com

B. tank bottom brick: The condition of the bottom brick is that the glass liquid temperature is low and the flow is weak. The tank bottom is now using the multi-layer compound bottom structure, usually the ground tiles use 300mm clay brick, then 25mm zircon sand or fused zirconia corundum ramming material are adopted above the clay bricks, the paving bricks adopt 75mm fused cast AZS block.

C. doghouse brick: doghouse is usually serious damaged as it is influenced by the erosion of powder and glass liquid, wear of material layer, and flame. Especially the corner of doghouse, so the corner brick generally adopts fused cast AZS block 41#. Except for the corner bricks, other parts can use PX casting fused cast AZS block 33#.

D. neck brick: the corner of neck adopts WS fused cast AZS block 41# which can strengthen the ability to resist erosion. The short neck crown and the neck part adopt high quality silica bricks.

E. cooling section: the temperature of glass liquid is lower than melting section, so the erosion is relatively lower, so fused cast AZS block 33# can be used in this part.

F. channel brick: usually adopt fused cast AZS block 33# or fused cast alumina block α-Al2O3.

G. regenerator chamber: top crown of regenerator usually adopts fused cast AZS block, direct bonded magnesia brick or silica brick. The top layers of side wall and partition wall use magnesia brick, middle layers use magnesia brick or low porosity clay brick, and bottom layers adopt low porosity clay brick.

Article source: http://fusedcastazs.com/news/64.html

Log in or register to post comments

61 Haier Rd Laoshan Qu Qingdao Shi Shandong Sheng , 266061 China

Via Fieramonti 1 04012 Cisterna di Latina LT Italy

No. 20 Binhe Road, High-tech Development Zone, Luolong Qu Luoyang Shi Henan Sheng , 471003 China

Fused Cast AZS Block Used In Different Parts Of Glass Furnace | glassonweb.com

Ceramic Fire Brick Changzhou Xingchen Industry Park Wujin Qu Changzhou Shi Jiangsu Sheng , 213119 China